A182 tilhører den amerikanske standard rustfrit stål smedegods til højtemperaturanlægsventiler og flangerørsfittings. A182 rustfrit stål, også kendt som ultra-low carbon rustfrit stål, er et alsidigt rustfrit stålmateriale, der er meget udbredt til fremstilling af trykbeholdere, udstyr og dele, der kræver gode omfattende egenskaber (korrosionsbestandighed og formbarhed).
| Handelsnavn |
karakter |
UNS # |
Smedede beslag |
| 304 |
F304 |
S30400 |
A182 / SA182 |
| 304L |
F304L |
S30403 |
A182 / SA182 |
| 304H |
F304H |
S30409 |
A182 / SA182 |
| 316 |
F316 |
S31600 |
A182 / SA182 |
| 316L |
F316L |
S31603 |
A182 / SA182 |
| 316H |
F316H |
S31609 |
A182 / SA182 |
| 321 |
F321 |
S32100 |
A182 / SA182 |
| 321H |
F321H |
S32109 |
A182 / SA182 |
| 347 |
F347 |
S34700 |
A182 / SA182 |
| 347H |
F347H |
S34709 |
A182 / SA182 |
| 317L |
F317L |
S31703 |
A182 / SA182 |
Kemiske egenskaber %
| karakter | C | Mn | P | S | Si | Ni | Cr | Mo |
| ASTM A182 F304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 8.0-11.0 | 18.0-20.0 | |
| ASTM A182 F304H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 8.0-11.0 | 18.0-20.0 | |
| ASTM A182 F304L | 0.03 | 2 | 0.045 | 0.03 | 1 | 8.0-13.0 | 18.0-20.0 | |
| ASTM A182 F304N | 0.08 | 2 | 0.045 | 0.03 | 1 | 8.0-10.5 | 18.0-20.0 | |
| ASTM A182 F304LN | 0.03 | 2 | 0.045 | 0.03 | 1 | 8.0-10.5 | 18.0-20.0 | |
| ASTM A182 F309H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 12.0-15.0 | 22.0-24.0 | |
| ASTM A182 F310 | 0.25 | 2 | 0.045 | 0.03 | 1 | 19.0-22.0 | 24.0-26.0 | |
| ASTM A182 F310H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 19.0-22.0 | 24.0-26.0 | |
| ASTM A182 F310MoLN | 0.03 | 2 | 0.03 | 0.015 | 0.4 | 21.0-23.0 | 24.0-26.0 | 2.0-3.0 |
| ASTM A182 F316 | 0.08 | 2 | 0.045 | 0.03 | 1 | 10.0-14.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F316H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 10.0-14.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F316L | 0.03 | 2 | 0.045 | 0.03 | 1 | 10.0-15.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F316N | 0.08 | 2 | 0.045 | 0.03 | 1 | 11.0-14.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F316LN | 0.03 | 2 | 0.045 | 0.03 | 1 | 11.0-14.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F316Ti | 0.08 | 2 | 0.045 | 0.03 | 1 | 10.0-14.0 | 16.0-18.0 | 2.0-3.0 |
| ASTM A182 F317 | 0.08 | 2 | 0.045 | 0.03 | 1 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 |
| ASTM A182 F317L | 0.03 | 2 | 0.045 | 0.03 | 1 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 |
| ASTM A182 F321 | 0.08 | 2 | 0.045 | 0.03 | 1 | 9.0-12.0 | 17.0-19.0 | |
| ASTM A182 F321H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 9.0-12.0 | 17.0-19.0 | |
| ASTM A182 F347 | 0.08 | 2 | 0.045 | 0.03 | 1 | 9.0-13.0 | 17.0-20.0 | |
| ASTM A182 F347H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 9.0-13.0 | 17.0-20.0 | |
| ASTM A182 F348 | 0.08 | 2 | 0.045 | 0.03 | 1 | 9.0-13.0 | 17.0-20.0 | |
| ASTM A182 F348H | 0.04-0.10 | 2 | 0.045 | 0.03 | 1 | 9.0-13.0 | 17.0-20.0 |
Mekaniske egenskaber
| karakter | Trækstyrke (Mpa) | Udbyttegrænse (Mpa) | Forlængelse (%) | Reduktion (%) |
| ASTM A182 F304 | 515 | 205 | 30 | 50 |
| ASTM A182 F304L | 485 | 170 | 30 | 50 |
| ASTM A182 F316 | 515 | 205 | 30 | 50 |
| ASTM A182 F316L | 485 | 170 | 30 | 50 |
| ASTM A182 F321 | 515 | 205 | 30 | 50 |
Beslag i rustfrit stål


Populære tags: astm a182 rustfrit stål rørfittings, Kina astm a182 rustfrit stål rørfittings producenter, leverandører
Et par af
Rørhætte i kulstofstålNæste
Excentrisk reduktionDu kan også lide
Send forespørgsel