Produktbeskrivelse
|
Længde af en side |
15 mm-500mm |
|
Vægtykkelse |
1mm-12mm |
|
Længde |
250 mm-12000mm |
|
Materiale |
SPHC,Q195,Q215,Q235,Q345,SAE1010,SAE1020 eller relativ |
|
Zink belægning |
220g/m2-800g/m2 |
|
Standard |
GB/T3091, EN10219, EN10210, ASTM A53 |
|
Certificering |
ISO9000 |
|
Teknik |
ERW, HFW |
|
Emballage |
Løs, plastik pakke, sorte strimler, GI strimler |
Specifikation for hult stålrør
| Størrelse | Størrelse | Tykkelse | Størrelse | Størrelse | Tykkelse |
| 25*25 | 30*20 | 1.2 | 1.8 | ||
| 1.3 | 2 | ||||
| 1.5 | 75*75 | 100*50 | 2.2 | ||
| 1.7 | 2.3 | ||||
| 1.8 | 2.5-4.0 | ||||
| 2 | 4.5-5.0 | ||||
| 2.2-2.3 | 5.5-5.75 | ||||
| 2.5-3.0 | 1.8 | ||||
| 30*30 | 1.5 | 2 | |||
| 1.7 | 2.2-2.3 | ||||
| 40*30 | 1.8 | 90*90 | 100*80 | 2.5-4.0 | |
| 40*25 | 2 | 120*60 | 4.5-5.0 | ||
| 40*20 | 2.2 | 5.5-5.75 | |||
| 2.3 | 7.5-7.75 | ||||
| 2.5-3.0 | 2 | ||||
| 2 | 120*80 | 2.2 | |||
| 60*30 | 2.2-2.3 | 100*100 | 150*50 | 2.3 | |
| 2.5-4.0 | 140*60 | 2.5-5.0 | |||
| 40*40 | 50*30 | 1.5 | 5.5-5.75 | ||
| 38*38 | 50*25 | 1.8 | 7.5-7.75 | ||
| 2 | 2.5 | ||||
| 2.2 | 2.75 | ||||
| 2.5-4.0 | 3 | ||||
| 1.5 | 120*120 | 160*80 | 3.25-5.0 | ||
| 1.7 | 5.5-7.0 | ||||
| 1.8 | 7.5-7.75 | ||||
| 50*50 | 60*40 | 2 | 2.5 | ||
| 2.2 | 2.75 | ||||
| 2.3 | 140*80 | 150*100 | 3 | ||
| 2.5-4.0 | 3.25-5.0 | ||||
| 4.25-5.0 | 5.5-7.0 | ||||
| 1.8 | 7.5-7.75 | ||||
| 2 | 2.5 | ||||
| 80*40 | 2.2-2.3 | 140*140 | 180*100 | 2.75 | |
| 60*60 | 70*50 | 2.5-4.0 | 150*150 | 200*100 | 3.0-4.0 |
| 4.25-5.0 | 4.5-7.0 | ||||
| 5.5-5.75 | 7.5-7.75 | ||||
| 1.8 | 3 | ||||
| 2 | 160*160 | 200*150 | 3.5 | ||
| 70*70 | 90*50 | 2.2 | 250*100 | 3.75 | |
| 80*60 | 2.3 | 4.0-7.75 | |||
| 2.5-4.0 | 300*100 | 3.5-3.75 | |||
| 4.5-5.0 | 200*200 | 250*150 | 4.0-5.75 | ||
| 5.5-5.75 | 220*220 | 220*150 | 7.5-7.75 | ||
| 2 | 250*125 | 9.5-11.75 | |||
| 2.2-2.3 | 400*100 | 3.5-3.75 | |||
| 80*80 | 2.5-3.0 | 250*250 | 250*200 | 4.5-7.25 | |
| 3.5-4.0 | 300*200 | 9.5-11.75 | |||
| 4.5-5.0 | 400*200 | 4.75-5.75 | |||
| 5.5-5.75 | 300*300 | 350*200 | 6.0-9.75 | ||
| 400*400 | 450*150 | 4.0-4.5 | 350*250 | 11.5-11.75 | |
| 280*280 | 450*200 | 4.75-5.0 | 350*300 | 4.75-5.0 | |
| 450*300 | 600*200 | 5.25-5.5 | 350*350 | 450*250 | 5.25-5.75 |
| 500*300 | 400*250 | 5.75-6.0 | 400*300 | 6.0-7.75 | |
| 400*350 | 500*350 | 6.5-11.75 | 500*200 | 8.0-11.75 |
Hule strukturelle sektion