A53 Gr.A Gr.B Gr.C ERW Stålrør
ASTM A53 er American Society for Testing and Materials (ASTM) standard for stålrør. Test- og materialestandard (ASTM) for stålrør til vand, gas, damp, aircondition og opvarmning og andre anvendelser af almindelige svejsede og sømløse kulstofstålrør. Standarden er opdelt i Standarden er opdelt i to typer: Type E (modstandssvejset rør) og Type S (sømløst rør).
Send forespørgsel
Chat nu
Produkt introduktion
ASTM A53 stålrør er ideelt til højtryksanvendelser. Derfor er ASTM A53ERW rør meget udbredt i industrier som olie- og gastransport. ASTM A53ERW rør er også meget udbredt i kulbrinte, bilindustrien, kedel og andre industrier.
A53 Rør kemisk sammensætning
| Grad | C | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|
| A | 0.25 | 0.95 | 0.05 | 0.045 | 0.4 | 0.4 | 0.15 |
| B | 0.3 | 1.2 | 0.05 | 0.045 | 0.4 | 0.4 | 0.15 |
A53 CS rørmekaniske egenskaber
| Grad | Trækstyrke | Udbyttestyrke |
|---|---|---|
| A | 330 | 205 |
| B | 415 | 240 |
A53 Steel Piep Størrelsestabel med lille diameter
| Udvendig diameter | Sch 5 | Sch 10 | Sch 40 | ||||
| tomme | mm | Tykkelse | Kg/mtr | Tykkelse | Kg/mtr | Tykkelse | Kg/mtr |
| 1/2" | 21.3 | 1.65 | 0.81 | 2.11 | 1.01 | 2.77 | 1.29 |
| 3/4" | 26.7 | 1.65 | 1.03 | 2.11 | 1.30 | 2.87 | 1.71 |
| 1" | 33.4 | 1.65 | 1.31 | 2.77 | 2.12 | 3.38 | 2.54 |
| 1 1/4" | 42.2 | 1.65 | 1.93 | 2.77 | 3.15 | 3.68 | 4.11 |
| 1 1/2" | 48.3 | 1.65 | 1.93 | 2.77 | 3.15 | 3.68 | 4.11 |
| 2" | 60.3 | 1.65 | 2.42 | 2.77 | 3.98 | 4.81 | 5.31 |
| 3" | 88.9 | 2.11 | 4.58 | 3.05 | 6.54 | 5.49 | 11.45 |
| 3 1/2" | 101.6 | 2.11 | 5.25 | 3.05 | 7.52 | 5.74 | 13.77 |
| 4" | 114.3 | 2.11 | 5.25 | 3.05 | 7.52 | 5.74 | 13.77 |
| 5" | 141.3 | 2.77 | 9.50 | 3.40 | 11.74 | 6.55 | 22.10 |
| 6" | 168.3 | 2.77 | 11.47 | 3.40 | 14.04 | 7.11 | 28.68 |
| 8" | 219.1 | 2.77 | 14.99 | 3.76 | 20.25 | 8.18 | 43.16 |
A53 ERW rør med stor diameter størrelsestabel
| OD | WT | ||||||||||||||||||
| tomme | mm | 8 5/8" | 219.1mm | 10 3/4" | 273.1 mm |
12 3/4" | 325.0 mm |
14" | 355.6 mm |
16" | 406.4 mm |
18" | 457.7 mm |
20" | 508.0 mm |
24" | 610 mm |
24 4/5" | 630.0 mm |
| 0.157 | 4.0 | ---- | --- | ||||||||||||||||
| 0.197 | 5.0 | --- | --- | --- | --- | --- | --- | --- | --- | ||||||||||
| 0.236 | 6.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||||||
| 0.276 | 7.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||||
| 0.315 | 8.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||
| 0.354 | 9.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||
| 0.394 | 10.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- |
| 0.133 | 11.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- |
| 0.492 | 12.5 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- |
| 0.551 | 14.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||||
| 0.630 | 16.0 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||||
| 0.689 | 17.5 | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | ||||||||
| 0.748 | 19.0 | --- | --- | --- | --- | --- | --- | --- | --- | ||||||||||
| 0.787 | 20.0 | --- | --- | --- | --- | --- | --- | ||||||||||||
GNEE ERW rør


Populære tags: A53 Gr.A Gr.B Gr.C ERW stålrør, Kina A53 Gr.A Gr.B Gr.C ERW stålrør producenter, leverandører
Et par af
API J55 API K55 svejset rørDu kan også lide
Send forespørgsel